Microstructure and properties of hard and wear resistant MMC coatings deposited by laser cladding J Nurminen, J Näkki, P Vuoristo International Journal of Refractory Metals and Hard Materials 27 (2), 472-478, 2009 | 321 | 2009 |
Corrosion properties of cold-sprayed tantalum coatings H Koivuluoto, J Näkki, P Vuoristo Journal of thermal spray technology 18, 75-82, 2009 | 131 | 2009 |
High performance corrosion resistant coatings by novel coaxial cold-and hot-wire laser cladding methods H Pajukoski, J Näkki, S Thieme, J Tuominen, S Nowotny, P Vuoristo Journal of Laser Applications 28 (1), 2016 | 48 | 2016 |
Analysis of the stress raising action of flaws in laser clad deposits MM Alam, AFH Kaplan, J Tuominen, P Vuoristo, J Miettinen, J Poutala, ... Materials & Design (1980-2015) 46, 328-337, 2013 | 41 | 2013 |
Comparison of laser cladding with powder and hot and cold wire techniques J Nurminen, J Riihimäki, J Näkki, P Vuoristo Pacific International Conference on Applications of Lasers and Optics, 2006 | 38 | 2006 |
Laser strip cladding for large area metal deposition J Tuominen, M Kaubisch, S Thieme, J Näkki, S Nowotny, P Vuoristo Additive Manufacturing 27, 208-216, 2019 | 32 | 2019 |
Microstructural and abrasion wear characteristics of laser-clad tool steel coatings J Tuominen, J Näkki, H Pajukoski, L Hyvärinen, P Vuoristo Surface Engineering 32 (12), 923-933, 2016 | 31 | 2016 |
Effect of minor elements on solidification cracking and dilution of alloy 625 powders in laser cladding J Näkki, J Tuominen, P Vuoristo Journal of Laser Applications 29 (1), 2017 | 27 | 2017 |
Wear and corrosion resistant laser coatings for hydraulic piston rods J Tuominen, J Näkki, H Pajukoski, J Miettinen, T Peltola, P Vuoristo Journal of Laser Applications 27 (2), 2015 | 20 | 2015 |
Laser cladding with 15 kW fiber laser J Tuominen, J Näkki, H Pajukoski, T Peltola, P Vuoristo, M Kuznetsov, ... Proceedings of the 13th NOLAMP Conference in Trondheim, 27-29, 2011 | 18 | 2011 |
Properties of alloy 625 claddings made with laser and CMT methods J Näkki Tampere University of Technology, 2018 | 16 | 2018 |
Recent developments in high power laser cladding techniques J Tuominen, J Näkki, H Pajukoski, T Peltola, P Vuoristo International Congress on Applications of Lasers & Electro-Optics 2012 (1 …, 2012 | 14 | 2012 |
Fatigue behavior of laser clad round steel bars J Tuominen, J Näkki, J Poutala, J Miettinen, T Peltola, P Vuoristo, ... Journal of laser applications 27 (1), 2015 | 13 | 2015 |
Surface pore initiated fatigue failure in laser clad components MM Alam, J Powell, AFH Kaplan, J Tuominen, P Vuoristo, J Miettinen, ... Journal of Laser Applications 25 (3), 2013 | 12 | 2013 |
Hot-wire cladding process studies J Nurminen, J Riihimäki, J Näkki, P Vuoristo International Laser Safety Conference, 2007 | 12 | 2007 |
Wood plastic composites with improved electrical and thermal conductivity R Rajan, J Näkki, R Layek, E Rainosalo Wood Science and Technology 55, 719-739, 2021 | 11 | 2021 |
High deposition rate laser cladding: recent advancements J Tuominen, J Naekki, H Pajukoski, T Peltola, P Vuoristo 5th Laser additive manufacturing workshop (LAM13), Housten, 2013 | 10 | 2013 |
Structure and corrosion behavior of cold-sprayed tantalum coatings H Koivuluoto, P Vuoristo, J Näkki Thermal Spray 2009: Expanding Thermal Spray Performance to New Markets and …, 2009 | 5 | 2009 |
The influence of powder parameters on laser cladding process J Nurminen, J Näkki, P Vuoristo International Congress on Applications of Lasers & Electro-Optics 2004 (1), P507, 2004 | 5 | 2004 |
A comparison of hot cracking sensibility of some alloy 625 powders on laser cladding J Näkki, J Tuominen, P Vuoristo International Congress on Applications of Lasers & Electro-Optics 2012 (1 …, 2012 | 4 | 2012 |